White Multi-Type Pipe Private Customization Yttria Stabilized Zirconia Tube Zro2 Grind Polished
Product Description
Zirconia material has advantages of high hardness, high strength, high tenacity, high wear resistance and good corrosion resistance which is widely applied in fields of ceramics, fire proofing material, machinery, electronic, photics, Aeronautics and astronautics, biology and chemicals and etc. Zirconia mill jar is particularly suitable for vertical stirring mill, horizontal rolling mill, vibration mill, and various high-wire-speed sanding stick pins, etc
1. Particularly suitable for vertical stirring mills, horizontal roller ball mills, vibrating mills and various high linear, speed pin- type sand mills.
2. For wet or dry ultrafine dispersion and grinding of pastes and powders without contamination.
3. Perfect grinding media with good flatness, smooth surface, bright,high density and high strength.
4. Wear and corrosion resistant product: coating, textile, pigment, dyeing.
5. High strength, high tenacity product: magnetic material, piezoelectric ceramics, dielectric ceramics.
6. Pollution prevention: medicine, food, cosmetics.
7. Ceramics: electronic ceramics, refractory ceramics, structural ceramics.
FAQ
1.Q: What is the size in your products?
A: Our common size is 0.1mm-100mm. We can also produce according to your request.
2.Q: What is your terms of delivery?
A: FOB, CFR, CIF.
3.Q: Can you accept small quantity sample order before production?
A: Yes, we can offer sample for your testing first before production, but the customers have to pay the courier cost.
4.Q: What is your production time?
A: Generally, it will take 5 to 30 days after receiving your advance payment. The specific delivery time depends on the items and the quantity of your order.
5.Q: What is your terms of payment?
A: T/T 30% as deposit, 70% balance against the copy of original B/L. Or 100% L/C at sight. We'll show you the photos of the products and the copy of original B/L before you pay the balance.
Features
Product Paramenters
Performance
|
Unit
|
Parameter
|
Component
|
Wt%
|
94.6% ZrO2, 5.2% Y2O3
|
Filled Density
|
Kg/l
|
3.5(φ5mm)
|
Density
|
g/cm3
|
5.95-6.00
|
Hardness
|
GPa
|
>11
|
Elasticity Modulus
|
GPa
|
200
|
Thermal conductivity
|
W/m.k
|
3
|
Coefficient of thermal Expansion
|
10*10-6/ºC(20-400)
|
9.6
|
Crush Strength
|
KN
|
≥20(φ7mm)
|
Bending toughness
|
MPam1/2
|
8
|